ITO Glass Substrates, 75 x 25 mm, PV and OLED
25 X 75 mm ITO patterned glass substrate, available with either modules or pixelated design. Perfect for use in OPV and OLED research.
The Pixelated Substrate System and Mini-Module Substrate System are designed to enable affordable scale-up. Alongside the Scale-Up Substrate Evaporation Masks, the substrates allow for larger devices and investigation of large-scale manufacturing techniques.
Datasheet
Size | 25 mm x 75 mm |
---|---|
Thickness | 1.1 mm |
Glass type | Polished soda lime, float glass |
Substrate coating | Fully oxidised ITO |
ITO thickness | 100 nm |
ITO resistance | 20 Ω/square |
Glass roughness | Less than 1 nm RMS (by AFM) |
ITO roughness | 1.8 nm RMS (by AFM) |
Dimensions
To the best of our knowledge the information provided here is accurate. However, Ossila assume no liability for the accuracy of this page. The values provided are typical at the time of manufacture and may vary over time and from batch to batch. All products are for laboratory and research and development use only, and may not be used for any other purpose including health care, pharmaceuticals, cosmetics, food or commercial applications.