PTAA for OFET Applications
PTAA, HTL material used to improve charge extraction in OLED/OFET devices
High quality polymer available with free shipping on qualifying orders
Methyl or fluoro substituted poly(triarylamines) (PTAAs) are electron rich with diphenylamine as the the backbone and substituted phenyl as side chains. Substituted PTAAs are originally used as hole transport layer (HTL) materials in OLED/OFET devices to improve charge extractions. PTAA can also act as electron blocking layer to reduce the chances of electron–hole recombination and energy loss in electronic devices. Fluorinated PTAA, 1F-PTAA and 2F-PTAA, can effectively downshift the HOMO levels of PTAA derivatives due to the electron deficiency of fluorine, resulting in an increase of VOC hence the power conversion efficiency (PCE) of the device.

PTAA from Ossila was used in the high-impact paper (IF 30.85), Multiply Charged Conjugated Polyelectrolytes as a Multifunctional Interlayer for Efficient and Scalable Perovskite Solar Cells, E. Jung et al., Adv. Mater., 2002333 (2020); DOI: 10.1002/adma.202002333.
A range of substituted poly(triarylamine)'s (PTAA's) for use with small molecules for solution-processed high-mobility films. While PTAA has a relatively modest mobility on its own, it has been gaining interest when used in conjunction with small molecules to provide the combination of good coating parameters and high mobility [1,2].
Note: We also have a PTAA family member (PTAA for perovskites) for perovskite solar cell applications.
Specifications
Name Batch number Mw Mn PDI MSDS |
4-Fluoro PTAA PE10-338-12 6,000 g/mol 4,020 g/mol 1.5 |
![]() |
Name Batch number Mw Mn PDI MSDS |
Dimethyl PTAA PE3-298-27B 6,312 g/mol 4,390 g/mol 1.4 |
![]() |
Name Batch number Mw Mn PDI MSDS |
2,4 Difluoro PTAA PE-338-8 4,712 g/mol 3,504 g/mol 1.34 |
![]() |
2,4 Difluoro PTAA Distibution Plot

Literature and References
Please note that Ossila has no formal connection to any of the authors or institutions in these references.
- Solvent and polymer matrix effects on TIPS-pentacene/polymer blend organic field-effect transistors Do Kyung Hwang et al., Journal of Materials Chemistry, V22, P5531-5537 (2012).
- Solution-Processed Small Molecule-Polymer Blend Organic Thin-Film Transistors with Hole Mobility Greater than 5 cm 2 /Vs J. Smith et al., Advanced Materials, V24, P2441-2446 (2012).
To the best of our knowledge the information provided here is accurate. However, Ossila assume no liability for the accuracy of this page. The values provided are typical at the time of manufacture and may vary over time and from batch to batch. All products are for laboratory and research and development use only, and may not be used for any other purpose including health care, pharmaceuticals, cosmetics, food or commercial applications.