PFN-FP-I
PFN-FP-I is a conjugated polymer electrolyte diiodide salt of PFN-FP. It is used either as an active layer material for blue OLEDs, or as an electron-interface layer material in organic electronic devices (including OLED, OPV and perovskite solar cells) to improve extraction efficiency.
Due to its strong polar ionic pendant groups, PFN-FP-I is soluble in methanol and water.
General Information
Full name | Poly[(9,9-bis(3'-(N,N-trimethylamino)propyl)-2,7-fluorene)- alt-1,4-phenylene] diiodide |
Synonyms | PFN-FP iodide; PFN-B-I |
Chemical formula | (C31H40N2I2)n |
CAS number | 1026670-72-3 |
Classification/Family | Conjugated polymers, Polymer electrolyte, Polyfluorenes, Electron interface layer materials, OLED, OPV, Perovskite materials, Water-soluble polymer materials |
Chemical Structure

MSDS Documentation
Pricing
Batch | Quantity | Price |
M2080A1 | 100 mg | £205.00 |
M2080A1 | 250 mg | £409.00 |
M2080A1 | 500 mg | £684.00 |
Literature and References
- Combination of Titanium Oxide and a Conjugated Polyelectrolyte for High-Performance Inverted-Type Organic Optoelectronic Devices, H. Choi et al., Adv. Mater., 23, 2759–2763 (2011); DOI: 10.1002/adma.201100266.
- Influence of polymeric electron injection layers on the electrical properties of solution-processed multilayered polymer light-emitting diodes, E. Itoh et al., Jpn. J. Appl. Phys. 55 02BB16 (2016); http://doi.org/10.7567/JJAP.55.02BB16.
- Huge enhancement of optical nonlinearities in coupled Au and Ag nanoparticles induced by conjugated polymers, L. Polavarapu et al., Appl. Phys. Lett. 100, 023106 (2012); https://doi.org/10.1063/1.3675911.
-
Enhanced Two-Photon Emission in Coupled Metal Nanoparticles Induced by Conjugated Polymers, Z. Guan et al., Langmuir, 26 (23), 18020–18023 (2010);
DOI: 10.1021/la103668k
To the best of our knowledge the information provided here is accurate. However, Ossila assume no liability for the accuracy of this page. The values provided are typical at the time of manufacture and may vary over time and from batch to batch. All products are for laboratory and research and development use only, and may not be used for any other purpose including health care, pharmaceuticals, cosmetics, food or commercial applications.