FREE shipping to on qualifying orders when you spend or more, processed by Ossila BV. All prices ex. VAT. Qualifying orders ship free worldwide! Fast, secure, and backed by the Ossila guarantee. It looks like you are visiting from , click to shop in or change country. Orders to the EU are processed by our EU subsidiary.

Product Code M122-100ml
Price $288 ex. VAT

Quality assured

Expert support

Volume discounts

Worldwide shipping

Fast and secure


High Conductivity PEDOT:PSS Formulation

Used for applications in OPV, OLED, and perovskite solar cells


Clevios™ PH 1000 PEDOT:PSS is designed for applications where high conductivity and optical transparency are required. The potential uses for high conductivity PEDOT:PSS formulations include replacements for ITO, semitransparent top electrodes in thin film electronics, top gate electrodes in FETs, and for use as a thick planarization layer on rough surfaces such as FTO. Sheet resistances as low as 300 Ω/square can be achieved with the addition of conductivity enhancement agents such as dimethyl sulfoxide and ethylene glycol.

Optical transparency PH 1000 PEDOT:PSS

Optical transparency

Ideal for interfacial layers

Versatile use for OPV, OLED and perovskite solar cells

Versatile use

Applications in OPV, OLED and perovskite solar cells

High quality PEDOT

High quality

Quality Formulation

High Conductivity PEDOT

High Conductivity

Tailored High conductivity

Technical Data

Solvent Water
Composition PEDOT/PSS (1:2.5 w/w)
CAS Number 155090-83-8
Solid Content 1.0 – 1.3 wt.%
Work Function 4.8 – 5.0 eV
Resistivity < 0.0012 Ω.cm
Conductivity High conductivity, 850 S/cm after the addition of 5% dimethyl sulfoxide (dried coating)
Particle Size Distribution D50 = 30 nm
Viscosity 15 – 60 mPa.s
pH Value 1.5 – 2.5
Packaging 100 ml of solution sealed in a light resistant bottle with temperature indicator
Storage 5 – 10 °C

Spin Speed Data

PH 1000 Spin Speed / Film ThicknessPH 1000 Spin Speed / Film Thickness

MSDS Document

PH 1000 MSDS SheetPH 1000 PEDOT:PSS MSDS Sheet


To the best of our knowledge the information provided here is accurate. The values provided are typical at the time of manufacture and may vary over time and from batch to batch. Products may have minor cosmetic differences (e.g. to the branding) compared to the photos on our website. All products are for laboratory and research and development use only.

Return to the top