FREE shipping to on qualifying orders when you spend or more, processed by Ossila BV. All prices ex. VAT. Qualifying orders ship free worldwide! Fast, secure, and backed by the Ossila guarantee. It looks like you are visiting from , click to shop in or change country. Orders to the EU are processed by our EU subsidiary.

Product Code M124-100ml
Price $288 ex. VAT

Quality assured

Expert support

Volume discounts

Worldwide shipping

Fast and secure


Aqueous PEDOT:PSS Formulation

Used for applications in OPV and perovskite solar cells


Clevios™ HTL Solar is an aqueous PEDOT:PSS formulation designed for use in thin film electronics as an interfacial material. The advantage of the HTL Solar formulation is its improved wetting properties, particularly in inverted OPV cells, compared to the other PEDOT:PSS formulations in our catalogue.

Increased Wettability HTL Solar PEDOT:PSS

Increased Wettability

Ideal for inverted OPVs and other thin films with wetting difficulties

Versatile use for OPV, OLED and perovskite solar cells

Versatile use

Applications in OPV, OLED and perovskite solar cells

High quality PEDOT

High quality

Quality Formulation

High Conductivity PEDOT

Tailored Conductivity

Relatively high conductivity, 0.1 – 1.0 S/cm

Technical Data

Solvent Water
Composition PEDOT/PSS (1:2.5 w/w)
CAS Number 155090-83-8
Solid Content 1.0 – 1.3 wt.%
Work Function 4.8 – 5.0 eV
Resistivity 1 – 10 Ω.cm
Conductivity Relatively high conductivity, 0.1 – 1.0 S/cm
Particle Size Distribution N/A
Viscosity 8 – 30 mPa.s
pH Value ~2
Packaging 100 ml of solution sealed in a light resistant bottle with temperature indicator
Storage 5 – 10 °C

Spin Speed Data

HTL Solar Spin Speed / Film ThicknessHTL Solar Spin Speed / Film Thickness

MSDS Document

HTL Solar MSDS SheetHTL Solar PEDOT:PSS MSDS Sheet


To the best of our knowledge the information provided here is accurate. The values provided are typical at the time of manufacture and may vary over time and from batch to batch. Products may have minor cosmetic differences (e.g. to the branding) compared to the photos on our website. All products are for laboratory and research and development use only.

Return to the top