AI 4083 PEDOT:PSS
CAS Number 155090-83-8
Organic Conductors, PEDOT:PSS (Poly(3,4-ethylenedioxythiophene) Polystyrene Sulfonate)
Quality assured
Expert support
Volume discounts
Worldwide shipping
Fast and secure
Popular Aqueous PEDOT:PSS Formulation
Used for applications in OPV, OLED, perovskite solar cells, and lighting
Clevios™ P VP AI 4083 is one of the most commonly used aqueous PEDOT:PSS formulations. Due to its deep work function it is often used for the matching of interfacial energy levels in thin film electronic devices. With a PEDOT:PSS ratio of 1:6, AI 4083 has low conductivity with relatively high resistance of 500 to 5000 Ω.cm. It has been widely used in organic and inverted PSCs and OLEDs as a hole transport material.
Deep Work Function
Matching interfacial energy levels
Versatile use
Applications in OPV, OLED and perovskite solar cells
High quality
Quality assured material
Low Conductivity
Tailored Low conductivity
Technical Data
Solvent | Water |
Composition | PEDOT/PSS (1:6 w/w) |
CAS Number | 155090-83-8 |
Solid Content | 1.3 – 1.7 wt.% |
Work Function | 5.0 – 5.2 eV |
Resistivity | 500 – 5000 Ω.cm |
Conductivity | Low conductivity, 0.0002 – 0.002 S/cm |
Particle Size Distribution | D90 = 100 nm; D50 = 80 nm |
Viscosity | 5 – 12 mPa.s |
pH Value | 1.0 – 2.0 |
Packaging | 100 ml of solution sealed in a light resistant bottle with temperature indicator |
Storage | 5 – 10 °C |
Spin Speed Data
Al 4083 Spin Speed / Film Thickness
MSDS Document
To the best of our knowledge the information provided here is accurate. The values provided are typical at the time of manufacture and may vary over time and from batch to batch. Products may have minor cosmetic differences (e.g. to the branding) compared to the photos on our website. All products are for laboratory and research and development use only.