HTL Solar 3 PEDOT Complex
Organic Conductors, PEDOT:PSS (Poly(3,4-ethylenedioxythiophene) Polystyrene Sulfonate)
Quality assured
Expert support
Volume discounts
Worldwide shipping
Fast and secure
Toulene-Based PEDOT Formulation
Used for applications in OPV and perovskite solar cells
Clevios™ HTL Solar 3 is a toulene-based PEDOT formulation using an alternative counter ionomer to PSS, allowing for the dispersion in toluene. HTL Solar 3 is ideal for use with materials, or in environments, that are water sensitive. Examples include in glove box environments or for use with perovskite inks or perovskite precursor materials.
Increased Wettability
Ideal for perovskite solar cells or with materials dissolved in or degraded by water.
Versatile use
ideal for use with water sensitive materials or environments
High quality
Quality Formulation
Low Conductivity
Low conductivity 0.002 – 0.2 S/cm
Technical Data
Solvent | Toluene |
Composition | PEDOT complex |
Solid Content | 1.5 – 2.5 wt.% |
Work Function | 4.4 – 4.8 eV |
Resistivity | 5 – 500 Ω.cm |
Conductivity | Low conductivity 0.002 – 0.2 S/cm |
Particle Size Distribution | N/A |
Viscosity | <30 mPa.s |
pH Value | N/A |
Packaging | 2 x 25 ml of solution sealed in light resistant bottles with temperature indicators |
Storage | 15 – 25 °C |
Spin Speed Data
HTL Solar 3 Spin Speed / Film Thickness
MSDS Document
To the best of our knowledge the information provided here is accurate. The values provided are typical at the time of manufacture and may vary over time and from batch to batch. Products may have minor cosmetic differences (e.g. to the branding) compared to the photos on our website. All products are for laboratory and research and development use only.