General Information

CAS number 507484-54-0
Chemical formula C12H5FN2O
Molecular weight 212.18 g/mol
Full name 2-[5(6)-Fluoro-3-oxo-2,3-dihydro-1H-inden-1-ylidene]malononitrile
Synonyms IC-F, 2-[5(6)-Fluoro-2,3-Dihydro-3-oxo-1H-inden-ylidene]-propanedinitrile
Classification / Family Malononitrile, Indanone, Monomer and intermediates, None-fullerene acceptors (NFAs), NFA-OSCs, printing electronics 

Chemical Structure

FIC - 2-((5)6-Fluoro-3-oxo-2,3-dihydro-1H-inden- 1ylidene)malononitrile CAS  507484-54-0
Chemical structure of FIC - 2-((5)6-Fluoro-3-oxo-2,3-dihydro-1H-inden- 1ylidene)malononitrile CAS 507484-54-0

Product Details

Purity >98% (by NMR)
Melting point n.a.
Appearance Off-white crystalline powder

MSDS Documentation

FIC MSDSFIC MSDS Sheet

Literature and Reviews

  1. A Well-Mixed Phase Formed by Two Compatible Non-Fullerene Acceptors Enables Ternary Organic Solar Cells with Efficiency over 18.6%, Y. Cai et al., Adv. Mater., 33 (33), 2101733 (2021); DOI: 10.1002/adma.202101733.
  2. Efficient Non-Fullerene Organic Photovoltaic Modules Incorporating As-Cast and Thickness-Insensitive Photoactive Layers, T. Zhang et al., Adv. Energy Mater., 8 (25), 1801387 (2018); DOI: 10.1002/aenm.201801387.
  3. An asymmetric acceptor enabling 77.51% fill factor in organic solar cells, J. Cao et al., Sci. Bull. 65, 1876–1879 (2020); DOI: 10.1016/j.scib.2020.08.004.
  4. High-Performance Additive-/Post-Treatment-Free Nonfullerene Polymer Solar Cells via Tuning Molecular Weight of Conjugated Polymers, Z. Li et al., Small, 14 (16), 1704491 (2018); DOI: 10.1002/smll.201704491.

To the best of our knowledge the information provided here is accurate. However, Ossila assume no liability for the accuracy of this page. The values provided are typical at the time of manufacture and may vary over time and from batch to batch. All products are for laboratory and research and development use only, and may not be used for any other purpose including health care, pharmaceuticals, cosmetics, food or commercial applications.

Return to the top