DTY6
DTY6 is another highly efficient non-fullerene acceptor from Y6 family with a highly conjugated and flat [1,2,5]thiadiazolo[3,4-e]thieno[2",3’':4’,5']thieno[2',3':4,5]pyrrolo[3,2-g]thieno[2',3':4,5]thieno[3,2-b]indole core centre.
Bearing two large decylteradecyl alky side chains, DTY6 is developed for large-area organic solar cells. Working together with polymers PBDB-TF-T1 (T1), PTO2, PClTO2. Non-fullerene acceptors DTY6, together with BTP-2F-12, TPT10-C8C12 and BTP-eC9 are considered to be green energy materials for their green solvents processability, i.e. in o-xylene or THF.
Polymer organic solar cells based on PM6:DTY6 processed in non-halogenated solvent o-xylene achieved power conversion efficiency of 16.1% with the following simple structure.
Device structure: indium tin oxide (ITO)/PEDOT:PSS/PM6:DTY6 (1:1.2, w/w, polymer weight concentration of 8 mg/mL)/PFNBr/Ag. [1]
Thickness (nm) | VOC (V) | JSC (mA cm-2) | FF (%) | PCEmax (%) |
110 ± 20 nm | 0.848 | 25.3 | 75.1 | 16.1 |
Chemical Structure

General Information
Purity | >99% (1H NMR) |
Full name | 2,2'-((2Z,2'Z)-((12,13-bis(2-decylteradecyl)-3,9-diundecyl-12,13-dihydro-[1,2,5]thiadiazolo[3,4-e]thieno[2",3’':4’,5']thieno[2',3':4,5]pyrrolo[3,2-g]thieno[2',3':4,5]thieno[3,2-b]indole-2,10-diyl)bis(methanylylidene))bis(5,6-difluoro-3-oxo-2,3-dihydro-1H-indene-2,1-diylidene))dimalononitrile |
Synonyms | BTP-4F-24, Y6-DT |
Chemical formula | C114H150F4N8O2S5 |
CAS number | n.a. |
Molecular weight | 1900.83 g/mol |
HOMO / LUMO | HOMO = -5.67 eV, LUMO = -4.04 eV [1] |
Absorption | λmax 716 nm (in o-xylene), 836 nm (in o-xylene processed film) |
Classification / Family | NFAs, n-type non-fullerene electron acceptors, Organic semiconducting materials, Low band-gap small molecule, Small molecular acceptor, Organic photovoltaics, Polymer solar cells, NF-PSCs. |
MSDS Documentation

Pricing
Batch | Quantity | Price |
M2274A1 | 50 mg | £199.00 |
M2274A1 | 100 mg | £303.00 |
M2274A1 | 250 mg | £606.00 |
M2274A1 | 500 mg | £1090.00 |
M2274A1 | 1 g | £1920.00 |
Literature and Reviews
- Single-Component Non-halogen Solvent-Processed High-Performance Organic Solar Cell Module with Efficiency over 14%, S. Dong et al., Joule 4 (9), 2004-2016 (2020); DOI: 10.1016/j.joule.2020.07.028.
To the best of our knowledge the information provided here is accurate. However, Ossila assume no liability for the accuracy of this page. The values provided are typical at the time of manufacture and may vary over time and from batch to batch. All products are for laboratory and research and development use only, and may not be used for any other purpose including health care, pharmaceuticals, cosmetics, food or commercial applications.