FREE shipping to on qualifying orders when you spend or more, processed by Ossila BV. All prices ex. VAT. Qualifying orders ship free worldwide! Fast, secure, and backed by the Ossila guarantee. It looks like you are visiting from , click to shop in or change country. Orders to the EU are processed by our EU subsidiary.

It looks like you are using an unsupported browser. You can still place orders by emailing us on info@ossila.com, but you may experience issues browsing our website. Please consider upgrading to a modern browser for better security and an improved browsing experience.

4CzPN-Ph

CAS Number 1469707-47-8

TADF Materials


Product Code M2375B1-250mg
Price £260 ex. VAT

4CzPN-Ph (4CzPNPh), a highly rigid carbazole based phthalonitrile derivative

Yellow emitter for highly efficient yellow and white TADF-OLED devices.


3,4,5,6-tetrakis(3,6-diphenylcarbazol-9-yl)- 1,2-dicyanobenzene (4CzPN-Ph), an iso-structure to 4CzTPN-Ph, has a fully substituted benzene ring with four bulky 3,6-diphenyl-9H-carbazoles and two ortho cyano groups at 1,2-positions.

Comparing with 4CzTPN-Ph, 4CzPN-Ph is structurally more hindered with all four diphenylcarbazolyl next to each other while four diphenylcarbazolyl are evenly separated in 4CzTPN-Ph. For this reason, 4CzTPN-Ph is relatively more conjugated is red-shifted in emission than 4CzPN-Ph.

4CzPN-Ph is a yellow emitter commonly used as a TADF dopant for highly efficient TADF devices. All TADF-based white organic light emitting diodes (WOLEDs) device with 4′-diphenylphosphinoylspiro[fluorene-9,9′-xanthene] (SFXSPO) as host, blue TADF material DMAC-DPS and yellow TADF material 4CzPN-Ph as the dopants, showed high device performance efficiencies with PE max of 40.6 lm/W, EQE max of 19.1%, and CE max of 50.5 cd/A.

General Information

CAS Number 1469707-47-8
Chemical Formula C104H64N6
Molecular Weight 1397.66 g/mol
Absorption λmax 
Fluorescence λem 
HOMO/LUMO HOMO = 5.5 eV, LUMO = 3.3 eV (ET = 2.81 eV) [1]
Full name 3,4,5,6-tetrakis(3,6-diphenylcarbazol-9-yl)- 1,2-dicyanobenzene
Synonyms 4CzPNPh, 3,4,5,6-tetrakis(3,6-diphenyl-9H-carbazol-9-yl)phthalonitrile
Classification / Family Carbazole derivatives, TADF yellow emitter materials, Phosphorescent organic light-emitting devices (PHOLEDs), TADF-OLEDs, organic electronics

Product Details

Purity Unsublimed >98.0%
Melting Point N/A
Colour Orange powder

Sublimation is a technique used to obtain ultra pure-grade chemicals. For more details about sublimation, please refer to the sublimed materials for OLED devices page.

Chemical Structure

4CzPNPh chemical structure, 3,4,5,6-tetrakis(3,6-diphenyl-9H-carbazol-9-yl)phthalonitrile, 4CzPN-Ph, CAS# 1469707-47-8
Chemical structure of 3,4,5,6-tetrakis(3,6-diphenylcarbazol-9-yl)- 1,2-dicyanobenzene  (4CzPN-Ph), CAS 1469707-47-8 

Device Structure(s)

Device Structure ITO/MoO3 (6 nm)/NPB (70 nm)/mCP (5 nm)/SFXSPO:4CzPNPh (20 nm, 5%wt.)/SFXSPO (5 nm)/TPBi (30 nm)/LiF(1 nm)/Al [1]
Colour Yellow yellow light emitting device
Max. EQE 9.9%
Max. Current Efficiency 27.9 cd/A
Max. Power Efficiency 25.0 lm W−1

 

Device Structure ITO/MoO3 (6 nm)/NPB (70 nm)/mCP (5 nm)/SFXSPO:4CzPNPh (20 nm, 5%wt.)/SFXSPO:DMAC-DPS (20 nm, 10%wt.)/SFXSPO (5 nm)/Bphen (30 nm)/LiF(1 nm)/Al [1]
Colour White white light emitting device
Max. EQE 19.1%
Max. Current Efficiency 50.5 cd/A
Max. Power Efficiency 40.6 lm W−1

 

Device Structure ITO/MoO3 (8 nm)/TAPC (40 nm)/5CzOXD: 4CzPNPh (8 wt% 20 nm)/BmPyPB (40 nm)/LiF (1 nm)/Al [2]
Colour Yellow yellow light emitting device
Max. EQE 17.1%
Max. Current Efficiency 50.6 cd/A
Max. Power Efficiency 64.7 lm W−1

 

Device Structure ITO/MoO3 (8 nm)/TAPC (40 nm)/mCP:5CzOXD:4CzPNPh  (66 : 33 : 1 wt%, 10 nm)/BmPyPB (40 nm)/LiF (1 nm)/Al [2]
Colour White white light emitting device
Max. EQE 9.9%
Max. Current Efficiency 20.7 cd/A
Max. Power Efficiency 33.4 lm W−1

Device Structure ITO/MoO3 (6 nm)/NPB (70 nm)/mCP (5 nm)/3-Sprio:4CzPNPh (5 wt%, 20 nm)/3-Sprio (5 nm)/TPBI (30 nm)/LiF (1 nm)/Al [3]
Colour White white light emitting device
Max. EQE 11.0%
Max. Current Efficiency 32.5 cd/A
Max. Power Efficiency 15.3 lm W−1

Pricing

 Grade Order Code Quantity Price
Unsublimed > 98% M2357B1 250 mg  £260
Unsublimed > 98% M2357B1 500 mg £420
Unsublimed > 98% M2357B1 1 g £660

MSDS Documentation

4CzPN-Ph MSDS4CzPN-Ph MSDS sheet

Literature and Reviews

  1. A Significantly Twisted Spirocyclic Phosphine Oxide as a Universal Host for High-Efficiency Full-Color Thermally Activated Delayed Fluorescence Diodes, J. Li et al., Adv. Mater. 28, 3122–3130 (2016); DOI: 10.1002/adma.201506286.
  2. Purely organic materials for extremely simple all-TADF white OLEDs: a new carbazole/oxadiazole hybrid material as a dual-role non-doped light blue emitter and highly efficient orange host, D. Zhang et al., J. Mater. Chem. C, 6, 3675-3682 (2018); DOI: 10.1039/c7tc04969b.
  3. Super rigid tris-spirobifluorenes: Syntheses and properties, L. Zhao et al., Chinese Chem. Lett., 32, 397-400 (2021); DOI: 10.1016/j.cclet.2020.02.001.
  4. Oligofluorene with multiple spiro-connections: its and their use in blue and white OLEDs, D. Xia et al., New J. Chem., 43, 3788 (2019); DOI: 10.1039/c8nj06135a.
  5. Flexible all fluorescence white organic light emitting device with over 22% EQE by stepped reverse intersystem crossing channels based on ternary exciplex, Z. Li et al., Org. Electronics, 91, 106076 (2021); DOI: 10.1016/j.orgel.2021.106076.
  6. Multi-dipolar Chromophores Featuring Phosphine Oxide as Joint Acceptor: A New Strategy toward High-Efficiency Blue Thermally Activated Delayed Fluorescence Dyes, C. Duan et al., Chem. Mater., 28, 16, 5667–5679 (2016); DOI: 10.1021/acs.chemmater.6b01691.
  7. Highly-efficient fully non-doped white organic light-emitting diodes consisting entirely of thermally activated delayed fluorescence emitters, J. Zhao et al., J. Mater. Chem. C, 6, 3226-3232 (2018); DOI: 10.1039/C8TC00639C.
  8. Recent advances in thermally activated delayed fluorescence for white OLEDs applications, C. Xue et al., J Mater Sci: Mater Electron 31, 4444–4462 (2020); DOI: 10.1007/s10854-020-03060-z.
Return to the top