4CzIPN-Me
CAS Number 1469703-61-4
Dopant Materials, Materials, Semiconducting Molecules, TADF Materials
A TADF yellow emitter
Used either as solo emitter in highly efficient TADF-OLEDs or an assistant dopant for TAF-OLEDs.
4CzIPN-Me, namely 2,4,5,6-Tetra(3,6-dimethylcarbazol-9-yl)-1,3-dicyanobenzene, is the methyl substituted 4CzIPN at 3,6-positions of the four carbazolyl units. Methyl groups at 3,6-positions will enhance the stability but also the solubility of the Carbazolyl benzonitriles. 4CzIPN-Me is the isomeric structure to 4CzPN-Me and 4CzTPN-Me.
By introducing an assistant dopant having a rather large kRISC~106, 4CzIPN-Me, both high electroluminescence efficiency and enhanced operational stability could be achieved in TADF assisted fluorescence (TAF-OLEDs). The state-of-the-art TAF-OLED technology uses a TADF molecule as an assistant dopant and a fluorescent molecule as an end emitter in a host matrix. The suppression of exciton annihilation was demonstrated via efficient and rapid triplet- singlet up conversion.
Electrogenerated chemiluminescence (ECL) study shows that the ECL intensity of 4CzIPN-Me decreases during voltage cycles due to the fact that polymerization happens on the carbazolyl moieties.
General Information
CAS Number | 1469703-61-4 |
Full Name | 2,4,5,6-Tetra(3,6-dimethylcarbazol-9-yl)-1,3-dicyanobenzene |
Synonyms | m4CzIPN, 2,4,5,6-Tetrakis(3,6-dimethyl-9H-carbazol-9-yl)-1,3-benzenedicarbonitrile, 2,4,5,6-tetrakis(3,6-dimethyl-9H-carbazol-9-yl)isophthalonitrile |
Chemical Formula | C64H48N6 |
Molecular Weight | 901.11 g/mol |
HOMO/LUMO | HOMO = 5.90 eV, LUMO = 2.81 eV [1] |
Classification / Family | Carbazole derivatives, Isophthalonitriles, TADF materials, Yellow dopant materials, Sublimed materials |
Chemical Structure
Product Details
Purity | Unsublimed >98.0% (1H NMR) |
Melting Point | N/A |
Appearance | Orange powder/crystals |
Device Structure(s)
Device Structure | ITO (100 nm)/HAT-CN (10 nm)/TAPC (30 nm)/6.3mol%-4CzIPN-Me:mCBP (30 nm)/T2T (10 nm)/Alq3 (55 nm)/LiF (0.8 nm)/Al (100 nm) [2] |
Colour | Greenish Yellow |
Max. Current Efficiency | 73 cd/A |
Max. EQE | 21% |
LT50@1,000 cd/m2 | 1472 h |
Device Structure | ITO (100 nm)/HAT-CN (10 nm)/TAPC (30 nm)/0.65mol%-TBRb:6.3mol%-4CzIPN-Me:mCBP (30 nm)/T2T (10 nm)/Alq3 (55 nm)/LiF (0.8 nm)/Al (100 nm) [2] |
Colour | Orange |
Max. Current Efficiency | 62 cd/A |
Max. EQE | 19.1% |
LT50@1,000 cd/m2 | 3775 h |
Pricing
Grade | Order Code | Quantity | Price |
---|---|---|---|
Unsublimed (>98.0% purity) | M2380 | 250 mg | £240 |
Unsublimed (>98.0% purity) | M2380 | 500 mg | £400 |
Unsublimed (>98.0% purity) | M2380 | 1 g | £640 |
MSDS Documentation
Literature and Reviews
- Efficiency loss processes in hyperfluorescent OLEDs: A kinetic Monte Carlo study, S. Gottardi et al., Appl. Phys. Lett., 114, 073301 (2019); DOI: 10.1063/1.5079642.
- Dual enhancement of electroluminescence efficiency and operational stability by rapid upconversion of triplet excitons in OLEDs, T. Furukawa et al., Sci Rep., 5, 8429 (2015); DOI: 10.1038/srep08429.
- High Efficiency in a Solution-Processed Thermally Activated Delayed-Fluorescence Device Using a Delayed-Fluorescence Emitting Material with Improved Solubility, Y. Cho et al., Adv. Mater., 26 (38), 6642-6646 (2014); DOI: 10.1002/adma.201402188.
-
A Novel Sterically Bulky Hole Transporter to Remarkably Improve the Lifetime of Thermally Activated Delayed Fluorescent OLEDs at High Brightness, T. Kamata et al., Chem. Euro. J., 24 (18), 4590-4596 (2017); DOI: 10.1002/chem.201705262.
-
Energy transfer processes in hyperfluorescent organic light-emitting diodes, E. Cho et al., J. Mater. Chem. C, 10, 4629-4636 (2022); DOI: 10.1039/D1TC05090G.
- Design of thermally activated delayed fluorescent sensitizers for high efficiency over 20% and long lifetime in yellow fluorescent organic light-emitting diodes, J. Ki met al., J. Mater. Chem. C, 8, 5265-5272 (2020); DOI: 10.1039/D0TC00178C.
-
Photophysical Properties and Efficient, Stable, Electrogenerated Chemiluminescence of Donor–Acceptor Molecules Exhibiting Thermal Spin Upconversion, R. Ishimatsu et al., Chem. Euro. J., 22 (14), 4889-4898 (2016); DOI: 10.1002/chem.201600077.
- Recent Progress of Singlet-Exciton-Harvesting Fluorescent Organic Light-Emitting Diodes by Energy Transfer Processes. S. Byeon et al., Adv. Mater., 31 (34), 1803714 (2019); DOI: 10.1002/adma.201803714.
Related Products
We stock a wide range of TADF materials available to purchase online. Please contact us if you cannot find what you are looking for.