Video: How to Make an OFET in Just 60 Seconds
This video shows how to make an OFET in just 60 seconds in order to perform OFET mobility measurements or to act as a chemFET (also called a chemical field effect transistor or OFET sensor). By using Ossila pre-fabricated test chips, five individual OFETs can be fabricated on one substrate to allow for multiple mobility measurements quickly and easily. The OFETs are fabricated simply by spin coating the organic semiconductor onto the test chip and wiping the edges clean.
Get going with OFETs and sensors
Get started making OFETs and sensors in your lab: contact our OFET support team directly or buy the test chips featured in the video.
Device Details Data
The device shown in the video produced average mobilities of >0.1 cm2/Vs and the polymer used was PBTTT in dichlorobenzene which was annealed under N2.