Video: How to Load the Low Density OFET Evaporation Stack
This video demonstrates how to load up the low density OFET stack ready to thermally evaporate (vacuum deposit) the source-drain contacts (compatible with most common OFET architectures such as top/bottom gate and top/bottom contacts).
Loading the evaporation stack consists of the below steps:
-
Loading the thin flexible mask onto the rigid lower support.
-
Loading the substrate support holder on top of the mask
-
Loading a substrate into the substrate support
-
Adding the magnetic sheet to hold the substrate and mask in close contact
-
Screwing the lid on to make a mechanically robust system ready for evaporation