2-Bromoanthracene
CAS Number 7321-27-9
Chemistry Building Blocks, Materials, Monomers, Non-Heterocyclic Building BlocksA useful building block for the construction of polycyclic aromatic hydrocarbon (PAH) anthracene
Used in OFETs and OLEDs devices.
Specifications | MSDS | Literature and Reviews
2-Bromoanthracene (CAS number 7321-27-9) is one of the many mono-brominated anthracene derivatives. Like its isomer 9-bromoanthracene, it is one of the useful building blocks for the construction of polycyclic aromatic hydrocarbon (PAH) anthracenes that are used in OFETs and OLEDs devices.
Top contact organic thin-film transistors (OTFTs) based on2-(anthracen-2-yl)tetracene (TetAnt), a p-type tetracene derivatives showed a hole mobility of up to 0.79 cm2 V-1 s-1. 2-(Anthracen-2-yl)-5-hexylthieno[3,2-b]thiophene (ASCTT) also achieved a high hole mobility of 0.1 cm2 V-1 s-1 and demonstrated the very efficient, trap-limited photoconductive behavior with a photoresponsivity up to 3370 A/W. OLED device based on a mixture of blue emitting 2-fluorenyl-2-anthracene and greenish-yellow emitting 2-anthryl-2-anthracence showed unusual solid-state white-light emission with the CIE coordinates (0.33, 0.34) at 10 V.
Anthracene building block
for the synthesis of OLED and organic photovoltaic materials
Worldwide shipping
Quick and reliable shipping
Substituted with a bromide group
for facile reactions
High purity
>98% Purity
General Information
| CAS Number | 7321-27-9 |
| Chemical Formula | C14H9Br |
| Full Name | 2-Bromoanthracene |
| Molecular Weight | 257.13 g/mol |
| Synonyms | Anthracene, 2-bromo- |
| Classification / Family | Anthracenes, Semiconductor synthesis intermediates, Low band gap polymers, OLED, OFETs, organic photovoltaics |
Chemical Structure
Product Details
| Purity | >98% (1H NMR) |
| Melting Point | Tm = 220 °C |
| Appearance | White to off-white powder/crystals |
MSDS Documentation
Literature and Reviews
- A small molecule composed of anthracene and thienothiophene devised for high-performance optoelectronic applications, Y. Jang et al., Dyes Pigm., 120, 30-36 (2015); DOI: 10.1016/j.dyepig.2015.04.004.
- Thermally stable organic thin film transistors based on 2-(anthracen-2-yl)tetracene, H. Yu et al., Org. Electron., 85, 105787 (2020); DOI: 10.1016/j.orgel.2020.105787.
- A Unique Blend of 2-Fluorenyl-2-anthracene and 2-Anthryl-2-anthracence Showing White Emission and High Charge Mobility, M. Chen et al., Angew. Chem. Intl. Ed., 56 (3), 722-727 (2017); DOI: 10.1002/anie.201608131.