A Variety of New Materials have been Added to Our Collection


Posted on Tue, Jul 19, 2016 by Lucy Roberts

This week's new molecular materials include C60 derivatives with higher solubility and higher open circuit voltage in solar cells than the standard electron acceptor material PCBM, in addition to popular phosphorescent bipolar host materials.

New products are continually being added to the catalogue, so make sure to keep a look out. You can also check out our brand new monomers catalogue for other available materials.  

Ir(ppy)2(bpmp)

Order Code: M761  

Ir(ppy)2(bpmp)Similarly to Ir(ppy)3, Ir(ppy)2(bpmp) is a phosphorescent green emitter. It is reported that the introduction of the para position methyl group to the pyridine nitrogen provides a twist and also an electron-donating effect. This raises the LUMO energy level of the complex, in addition to the triplet energy level, resulting a blue shift in the emission.  

View the product page for Ir(ppy)2(bpmp).

CAS number 1215692-34-4
Chemical formula C40H30IrN3
Molecular weight 744.90 g/mol
Absorption λmax = 212 nm, 244 nm, 285 nm

 

26DCzPPy

Order Code: M771

26DCzPPyWith combination of a carbazole electron donor with a high triplet energy and a pyridine electron acceptor with a high electron affinity, 26DCzPPy is one of the most popular bipolar charge transport layer host materials used in OLEDs.

View the product page for 26DCzPPy.

CAS number 1013405-24-7
Chemical formula C41H27N3
Molecular weight 561.67 g/mol
HOMO/LUMO
HOMO = 6.05 eV, LUMO = 2.56 eV 

 

35DCzPPy

Order Code: M781


35DCzPPy35DCzPPy
is an isomer of 26DCzPPy, differing in the position of the functionalisations of the central pyridine ring. 35DCzPPy is more electron rich, so 26DCzPPy has a better balanced hole and electron injection and transport than 35DCzPPy.

View the product page for 35DCzPPy.

CAS number 1013405-25-8
Chemical formula C41H27N3
Molecular weight 561.67 g/mol
HOMO/LUMO
HOMO = 6.18 eV, LUMO = 2.75 eV

 

[60]PCBH

Order Code: M821

 

[60\PCBH[60]PCBH, Phenyl-C61-butyric acid hexyl ester is a fullerene derivative of C60 that is more soluble than PCBM. This makes it more desirable when higher concentrations of the electron acceptor material are required when making photovoltaic devices. 

View the product page for [60]PCBH.

CAS number 850807-50-0
Chemical formula C77H24O2
Molecular weight 981.01 g/mol
HOMO/LUMO No data available; comparable to PCBM (HOMO 6.1 = eV, LUMO = 3.7 eV)

 

[60]IPB

Order Code: M831

[60]IPB[60]IPB is also a fullerene derivative of C60 which is used as an electron acceptor material in photovoltaic cells. In comparison with PCBM and its derivatives, [60]IPX fullerenes (where X is either B (butyl), H (hexyl) or O (octyl)) give about 50 mV higher open circuit voltage (VOC). 

View the product page for [60]IPB.

CAS number 1705592-13-7 (1883713-20-9)
Chemical formula C76H20O2
Molecular weight  964.97 g/mol
HOMO/LUMO No data available; comparable to PCBM (HOMO 6.1 = eV, LUMO = 3.7 eV)