New I201 Perovskite Precursor Ink (for Inert Processing Demonstrates) 11.8% Efficiency

Posted on Tue, Feb 24, 2015

Following on from the success of our first perovskite precursor ink, we have developed a new perovskite ink, I201, which is is designed to be processed in an inert (nitrogen atmosphere) and which has already shown 11.8% PCE in our labs.

Data, processing recipe and video demonstrations are now available from the product page.