Unpatterned ITO/Glass Substrates for OLEDs/OPVs



Unpatterned ITO Substrate Unpatterned ITO substrates. Useful for a variety of experimental techniques including STM, conductive AFM and spectroscopy.

Substrate size: 20 mm x 15 mm
ITO coverage: complete
ITO resistance: 20 Ohm / square
Packaging: Stacks of 20 separated by cleanroom paper
Larger area substrates are also available in:

• 50 mm x 50 mm x 0.7 mm

ITO resistance: 20 Ohm / square

Order codeDesignQuantityPrice
S111 20 mm x 15 mm 100 £149
S112 20 mm x 15 mm 1000 £999
S113 50 mm x 50 mm x 0.7 mm 100 £299