Pre-patterned ITO/Glass Substrates for OPV/OLED Testing



Prepatterned substrate Pre-patterned ITO substrates for OPV/OLED testing. Use with our cathode deposition mask (E111) to create individual pixels.


Order codeQuantityPrice
S101 100 £550
S102 1000 £3500




Other products you may be interested in...

Encapsulation Epoxy
Electrical Connection Legs
Substrate packs
Encapsulation epoxy
Electrical connection legs
Substrate packs


Printable HTML Datasheet Adobe PDF


Ossila's ITO substrates can be used to prepare organic photovoltaic cells and organic light emitting diodes. They are manufactured from commercial grade ITO used in the flat panel display industry in order to endure high consistency and very low defect rates. Each substrate has six ITO fingers which when used with an Ossila evaporation shadow masks creates six independent devices with dimensions of 1.5 mm x 3 mm. An additional cathode strip allows easy connection of both anodes and cathodes by attachment of electrical legs. The substrates are packed in stacks of 20 individually separated by pieces of cleanroom paper. A simple cleaning procedure then provides a clean and hydrophilic surface perfect for spinning PEDOT:PSS.


Completed prepatterned substrate

Completed Device



Substrate dimensions20 mm x 15 mm
Pixel dimensions(with cathode) 3 mm x 1.5 mm (4.5 mm^2)
Glass Type Polished Soda Lime, Float
Glass Thickness 0.7 mm
Substrate Coating Fully Oxidized ITO
ITO Thickness 100 nm
ITO Resistance 20 Ohm


Use:To prepare the substrates for use we recommend cleaning in a solution of hot sodium hydroxide (NaOH) which will both help remove any dust and also provide a hydrophilic surface without the need for a plasma or UV clean (note that some materials/solutions particularly close to the wetting envelope may still benefit from a plasma clean). We use the following cleaning routine for OPVs and OLEDs, however please note that exact times will depend upon the power and temperature of the sonic bath and that excessive sonication can also increase the resistance of the ITO surface.

  • Sonicate in 10% NaOH solution for 5 mins using a hot bath
  • Rinse thoroughly in hot water
  • Sonicate in fresh 10% NaOH solution for 5 mins using a hot bath
  • Rinse thoroughly in hot water
  • Store immersed in water until required
  • N2 blow dry



Optical absorption with and without PEDOT:PSS
Prepatterned ITO Substrate Optical Absorption






To the best of our knowledge the information provided here is accurate. However, Ossila assume no liability for the accuracy of this information. The values provided here are typical at the time of manufacture and may vary over time and from batch to batch.





Search
Loading
Ossila Orders

Simply phone, fax or email your purchase order to us

All prices subject to VAT where applicable

Shipping and Returns

Terms and conditions apply

If applicable, please provide your VAT registration number when placing an order