TIPS pentacene
|
6,13-bis(triisopropylsilylethinyl)pentacene commonly known as TIPS pentacene. Now in stock for immediate dispatch.
A high purity TIPS pentacene for use in organic field-effect transistors (OFETs). In stock for immediate delivery to academic institutions in Europe and selected other geographical areas outside of North America. TIPS pentacene has become widespread as a high performance small molecule for OFET applications with a mobility in excess of 1 cm2/Vs having being achieved in the literature. It has excellent solubility in a range of common organic solvents and a good ambient stability making it easy to process into devices. This Ossila TIPS pentacene has been produced with a purity of >99.5% and trace metal below 5 PPM.
Please note that TIPS Pentacene is unavailable to buyers in the USA. Any incoming orders from the USA for TIPS Pentacene will not be processed. |
| Other products you may be interested in... |
|
Printable HTML MSDS |
Datasheet |
|
6,13-bis(triisopropylsilylethinyl)pentacene commonly known as TIPS pentacene
Cas no: 373596-08-8

Generic Properties
| Appearance | Dark Blue Solid |
| Molecular Formula | C44H54Si2 |
| Molecular Weight | 639.07 |
| Solvents | Anisole, butylbenzene, chlorobenzene, chloroform, dichlorobenzene, tetrahydrofuran, toluene, xylene |
| Recommended solvent | Toluene |
| Recommended concentration | 10 mg/ml (drop cast / spin cast) |
Batch Specific Properties
| Batch Number | 49955 |
| Purity (HPLC) | >99.5% |
| Trace metal analysis (ICP OES) | Na, K, Sn, Mg, Ca, Zn, Al, Ba all < 5 PPM |
| DSC Endotherm melt onset | 255°C |
| DSC Exotherm onset | 260°C |
DSC trace
NMR trace
Crystallisation Images
Images below taken of thin films of TIPS pentacene deposited by spin casting and drop casting from toluene (10 mg/ml) on SiO2 showing the strong crystallisation behaviour especially in slow dried films.