PEDOT:PSS (AI 4083 for spin coated devices)




PEDOT:PSS
Heraeus Clevios™ PH1000 Clevios P VP AI 4083 - one of the most commonly used PEDOT:PSS formulations for spin coated OPVs and OLEDs. Spins to ~40 nm at 5000 rpm.

Resistivity: 500-5000 ohm cm
Solid content: 1.3 to 1.7%
Na content: 400 ppm maximum
Sulfate content: 40 ppm maximum
Viscosity: 5-12 mPa s
PEDOT:PSS ratio: 1:6
Work funtion: ~5.2 eV
Usage: <100 μl per standard (20 mm x 15 mm) substrate.
Cas no: 155090-83-8

For information on usage please see our OLED/OPV fabrication video and written fabrication guide or please contact us for more information.

Order codeQuantityPrice
M121 100 ml £149




Other products you may be interested in...

P3HT
PEDOT:PSS PH1000
Measurement aperture mask
P3HT
PEDOT:PSS PH1000
Measurement aperture mask





Search
Loading
Ossila Orders

Simply phone, fax or email your purchase order to us

All prices subject to VAT where applicable

Shipping and Returns

Terms and conditions apply

If applicable, please provide your VAT registration number when placing an order