P3HT
|
Regioregular poly(3-hexylthiophene-2,5-diyl). Commonly known as P3HT.
Ossila provides a range of P3HT with different molecular weights and regioregularities for a variety of research purposes. Produced by Merck KGaA under the Lisicon® brand this high quality P3HT collection allows a wider range of science and engineering to be undertaken than by using a single P3HT. |
The highest regioregularity P3HT (M101, RR=96.6%) produces highly crystalline films and is recommended for OFETs, nanofibril formation and fast drying OPVs at the thin interference peak (~90 nm). However, the exceptionally high regioregularity of this P3HT means that gelling and surface roughness can be an issue for slow-drying thick-film OPVs (>200 nm). Lower molecular weight and regioregularity P3HT is recommended for inkjet and other large area or slow drying deposition techniques where gelling/aggregation and surface roughness need to be avoided.
All the P3HT below is highly soluble (~50 mg/ml) in chlorinated solvents such as chloroform, chlorobenzene, dichlorobenzene and trichlorobenzene. The intermediate and lower molecular weight P3HT materials are recommended for use with non-chlorinated solvents such as xylene, toluene and THF due to their increased solubility.
CAS no: 104934-50-1
The below P3HT is in stock for immediate dispatch:
|
The following P3HT is also available upon request with prices from £499. Please contact us to for formal quotations, availability and/or delivery schedules (usually 1 to 2 weeks).
|